HW-101 Lever/Fessin up time

Brian Wood brianmwood at EMAIL.MSN.COM
Sun Jan 7 17:59:50 EST 2001


I saw some "casting resin" at The Home Depot that might work, too.

Brian

----- Original Message -----
From: MIKE SOUHRADA <wb9iog at REVEALED.NET>
To: <HEATH at LISTSERV.TEMPE.GOV>
Sent: Saturday, January 06, 2001 9:02 PM
Subject: Re: HW-101 Lever/Fessin up time


> KISS principle. I used modeling plaster to form a new lever knob
> from a good one with the metal insert removed.
> I used craft paints for an almost perfect match. For the material
> I used J&B Weld, that's really neat stuff. Was concerned about strength
> but it turned out very well and appeared to be as strong if not
> stronger than the original material.
> The insert went in just fine as there was enough give in J&B Weld to
> not crack.

Listserver Subscription:listserv at listserv.tempe.gov - "subscribe heath 'name' 'call'"